In the steelmaking process, after the converter smelting is completed, the molten steel is poured into the ladle through the converter tap;

Various alloy materials need to be added during the tapping process to achieve precise adjustment of the composition of the molten steel; the alloy materials are generally introduced from the rotating chute to the ladle when the tapping volume of the converter reaches 20%-30%, and the tapping volume Add up when it reaches 70%-80%;

During the tapping process, in order to make the alloy material melt in time and ensure the uniformity of the molten steel alloy composition, the blanking center of the rotating chute must be aligned with the molten steel injection center.

In order to achieve this goal, the current steel mill rotary chute devices adopt fixed stoppers to control the blanking position of the rotary chute body. The rotary chute device includes a rotary chute body, a shell, a rotating gear plate, a limit baffle, and a discharge Position limiter and parking position limiter, the limit baffle is fixed on the rotating gear plate, the discharge position limiter and the parking position limiter are fixed on the shell.

The electric control system and PLC control system are installed in the converter tapping operation room to realize the rotation of the rotating gear plate and drive the rotation of the rotating chute. When the limit baffle rotates from the stop position stopper position to the discharge position stopper position, it rotates The gear plate stops automatically. At this time, the blanking position of the rotating chute should be aligned with the molten steel injection center to complete the addition of alloy materials.

In the actual production process, it often happens that after the rotating chute reaches the discharge position, the blanking center and the molten steel injection center are not aligned, causing the alloy material to be unable to melt in time after being added to the ladle, and the molten steel alloy composition is uneven, and the molten steel alloy The composition hit rate is low, especially when the alloy material is added more, the unevenness of the molten steel alloy composition is particularly prominent.

2 solution

The new converter alloy material developed by Handan Iron and Steel is added to the rotating chute device, which can quickly and accurately control the position of the rotating chute blanking, and can realize the timely adjustment of the rotating chute blanking position, so that the blanking position can be automatically adjusted to the molten steel injection center. Aligned.

This kind of converter alloy material is added to the rotating chute device, which includes the rotating chute body, the shell, the rotating gear plate, the limit baffle, the discharge position limiter and the parking position limiter. The limit baffle is fixed on the rotating gear plate, The improvement is: it also includes a limiter control component fixed on the housing, the limiter control component is provided with a chute, and the discharge position limiter and the parking position limiter are installed on the limiter control component In the chute. The parking position limiter is fixed at one end of the chute of the limiter control part, and the discharge position limiter is in a sliding connection with the chute of the limiter control part.

The limiter control component is an arc-shaped plate with a chute. The curvature of the arc-shaped plate is the same as that of the shell. The width of the chute is 2-5mm greater than the width of the discharge position limiter, and the length is greater than or equal to the circle. 1/4 of the circumference of the shell.

The working process of adding this kind of converter alloy material to the rotating chute device is as follows: press the "discharge position" button before tapping, and the rotating chute body will start to rotate under the drive of the rotating sprocket. When the limit baffle on the rotating sprocket rotates When the position of the discharge position limiter is reached, the rotating gear plate automatically stops, and the blanking position center of the rotating chute body is pre-aligned with the molten steel injection center. When it is found to be misaligned, the discharge position limiter is moved Align the position in the chute; when the converter is tilted down to an inclination angle of 20%-30% of the tapping volume, press the "discharge level" button, the alloy silo will automatically open, and discharge through the rotating chute. During the process, the blanking center of the chute will always be aligned with the molten steel injection center to ensure that the alloy material falls in the impact area of ​​the molten steel injection.

3 use effect

The device realizes the timely movement of the discharge position limiter in the chute by adding a limiter control board. When it is found that the blanking center of the rotating chute and the molten steel injection center are not in the same position and cannot be centered, the discharge position is manually adjusted. The material level limiter can ensure the centering of the blanking center of the rotating chute and the molten steel injection center, which solves the problems of slow alloy melting speed, uneven melting and large composition fluctuations during the alloy feeding process, and improves the composition of the molten steel alloy. The hit rate. The device has a simple structure and significant effects, and is suitable for popularization and application in various iron and steel enterprises.

4 Economic and social benefits

4.1 Economic benefits

1) For products produced by the new technology, the average monthly scrap steel products that avoid composition fluctuations and composition segregation are about 200 tons, 600 tons of downgraded products, the price of first-class products is 3000 yuan/ton, and the price of scrap steel is 1000 yuan/ton. After the first-class product is downgraded, the price will be reduced by 150 yuan per ton, and the average monthly loss will be reduced: 200 tons × 2,000 yuan/ton + 600 tons × 150 yuan/ton = 490,000 yuan, an annual benefit of 490,000 yuan/month × December=588 Ten thousand yuan.

2) Through the use of a new type of converter alloy material rotating chute device, the overall technological level of the converter production line has been improved. After the product quality is stable, the monthly average output will increase by 1,000 tons, creating an additional benefit of about 150 yuan per ton, and the annual social benefit: 1,000 tons / Month × December × 150 yuan / ton = 1.8 million yuan.

3) Reduce equipment consumption and maintenance costs by 29,000 yuan/month, and reduce annual costs by 29,000 yuan/month×12 months=348,000 yuan.

The total of the three items: 588+180+34.8=8.028 million yuan/year.

4.2 Social benefits

The successful application of the new converter alloy material added to the rotary chute device developed by Handan has filled the gap in the technical field of domestic converter alloy material addition method control, improved the alloy melting speed and uniformity during the alloy feeding process, and can stably improve the uniformity of the converter smelting composition Performance, thereby improving the hit rate of molten steel alloy components and increasing profitability.


Please keep the source and address of this article for reprinting: Technological Innovation to Improve the Homogeneity of Converter Smelting Composition


Minghe Die Casting Company are dedicated to manufacture and provide quality and high performance Casting Parts(metal die casting parts range mainly include Thin-Wall Die Casting,Hot Chamber Die Casting,Cold Chamber Die Casting),Round Service(Die Casting Service,Cnc Machining,Mold Making,Surface Treatment).Any custom Aluminum die casting, magnesium or Zamak/zinc die casting and other castings requirements are welcome to contact us.

ISO90012015 AND ITAF 16949 CASTING COMPANY SHOP

Under the control of ISO9001 and TS 16949,All processes are carried out through hundreds of advanced die casting machines, 5-axis machines, and other facilities, ranging from blasters to Ultra Sonic washing machines.Minghe not only has advanced equipment but also have professional team of experienced engineers,operators and inspectors to make the customer’s design come true.

POWERFUL ALUMINUM DIE CASTING WITH ISO90012015

Contract manufacturer of die castings. Capabilities include cold chamber aluminum die casting parts from 0.15 lbs. to 6 lbs., quick change set up, and machining. Value-added services include polishing, vibrating, deburring, shot blasting, painting, plating, coating, assembly, and tooling. Materials worked with include alloys such as 360, 380, 383, and 413.

PERFECT ZINC DIE CASTING PARTS IN CHINA

Zinc die casting design assistance/concurrent engineering services. Custom manufacturer of precision zinc die castings. Miniature castings, high pressure die castings, multi-slide mold castings, conventional mold castings, unit die and independent die castings and cavity sealed castings can be manufactured. Castings can be manufactured in lengths and widths up to 24 in. in +/-0.0005 in. tolerance.  

ISO 9001 2015 certified manufacturer of die cast magnesium and mold manufacturing

ISO 9001: 2015 certified manufacturer of die cast magnesium, Capabilities include high-pressure magnesium die casting up to 200 ton hot chamber & 3000 ton cold chamber, tooling design, polishing, molding, machining, powder & liquid painting, full QA with CMM capabilities, assembly, packaging & delivery.

Minghe Casting Additional Casting Service-investment casting etc

ITAF16949 certified. Additional Casting Service Include investment casting,sand casting,Gravity Casting, Lost Foam Casting,Centrifugal Casting,Vacuum Casting,Permanent Mold Casting,.Capabilities include EDI, engineering assistance, solid modeling and secondary processing.

Casting Parts Application Case Studies

Casting Industries Parts Case Studies for: Cars, Bikes, Aircraft, Musical instruments, Watercraft, Optical devices, Sensors, Models, Electronic devices, Enclosures, Clocks, Machinery, Engines, Furniture, Jewelry, Jigs, Telecom, Lighting, Medical devices, Photographic devices, Robots, Sculptures, Sound equipment, Sporting equipment, Tooling, Toys and more. 


What Can we help you do next?

∇ Go To Homepage For Die Casting China

→Casting Parts-Find out what we have done.

→Ralated Tips About Die Casting Services


By Minghe Die Casting Manufacturer |Categories: Helpful Articles |Material Tags: , , , , , ,Bronze Casting,Casting Video,Company History,Aluminum Die Casting |Comments Off

MingHe Casting Advantage

  • Comprehensive Casting design software and skilled engineer enables sample to be done within 15-25 days
  • Complete set of inspection equipment & quality control makes excellent Die Casting products
  • A fine shipping process and good supplier guarantee we can always deliver Die Casting goods on time
  • From prototypes to end parts, upload your CAD files, fast and professional quote in 1-24 hours
  • Wide-ranging capabilities for designing prototypes or massive manufacturing end use Die Casting parts
  • Advanced Die Casting techniques (180-3000T Machine,Cnc Machining, CMM) process a variety of metal & plastic materials

HelpFul Articles

Rare earth can effectively improve the toughness of cast steel

As we all know, adding an appropriate amount of rare earth elements to steel materials will have a s

Technological Innovation to Improve the Homogeneity of Converter Smelting Composition

In the steelmaking process, after the converter smelting is completed, the molten steel is poured in

"Alkali" and "Magnesium" to improve pellet performance

Oxidized pellets have good mechanical strength and metallurgical properties, and have become an indi

Analysis and Improvement of Common Defects of Valve Castings

1. Stoma     This is a small cavity formed by the gas that has not escaped during the solidificatio

The Measures To Improve Continuous Casting Tundish Life

The life of the continuous casting tundish determines the index of the number of continuous casting

The Improvement Method Of Mold Performance

In addition to the reasonable coordination of the matrix with sufficiently high strength and toughne

The Measures To Improve The Life Of Aluminum-Magnesium Alloy Die Casting Mold

As an important processing equipment, aluminum-magnesium alloy die-casting molds have a direct impac

5 Major Links Need To Be Controlled To Improve Mold Life

Including mold production plan formulation, mold design, process formulation, workshop task assignme

How to greatly improve the quality of bearing steel by super fast cooling after rolling

To a certain extent, the quality of bearings restricts the speed and progress of the national econom

How to improve the service life of the intermediate frequency furnace?

Improving the service life of the induction furnace body is the goal pursued by every foundry worker

Three Keys To Improve The Spheroidization Rate And Ductile Iron Graphite Roundness

Rare earth has two beneficial effects in molten iron: one is desulfurization and degassing, playing

The Measures To Improve High Anti-Collapse Casing Life

The problem of casing damage seriously restricts oil and gas production, reduces the production life

The Measures To Improve The Quality Of Carbon-Manganese Steel Rudder Stock

The rudder stock is the shaft on which the rudder blades rotate. The rudder blades are rotated by th

The Methods To Improve Electromagnetic Pure Iron Wear Resistance

Electromagnetic pure iron is a widely used soft magnetic material. It has high magnetic induction an

The Measures To Improve The Quality Of SWRCH22A Wire Rod

SWRCH22A is a kind of hot-rolled non-twist and controlled cooling wire rod. Mainly used to manufactu

Die casting release agent can improve production efficiency and quality problems

The function of die-casting release agent is to improve the production efficiency of castings and pr

The Improvement Of Current Shell Making Process In Investment Casting

The inoculation amount is generally determined according to the metallographic structure of the prod

How to improve the casting process measures of the spheroidization rate

The spheroidization level of domestic ordinary spheroidal graphite cast iron castings is required to

How Does Silicon Carbide Improve The Quality Of Castings?

The addition of silicon carbide can prevent the precipitation of carbides, increase the amount of fe

Process Improvement For Loose Thin-Walled Castings And Under-Casting Defects

The wall thickness of the regulating piece and sealing piece of high-temperature alloy castings is c

Using Oxygen And Nitrocarburizing To Improve Aluminium Die Performance

Oxygen and nitrocarburizing treatment can be carried out in a pit carburizing furnace, using liquid

Improvement and optimization of ultra-low carbon martensitic stainless steel smelting process

Ultra-low carbon martensitic stainless steel (06Cr13Ni46Mo and 06Cr16Ni46Mo) is an important materia