How To Calculate Pressure Die Casting Tonnage

How To Calculate Pressure Die Casting Tonnage

Calculation Formula The calculation formula for the selection of die-casting machine: Die-casting machine clamping force (t) = 1.4 * casting projected area * ratio of the projected area of ​​the die ...

The Key Points Of Aluminum Alloy Die Casting Design

The Key Points Of Aluminum Alloy Die Casting Design

An excellent die casting designer should be familiar with the die casting process and the production process of die casting, so that the design of die casting conform to the most simple production and the most convenient production operation requirements. Die casting design is the most fundamental l ...

High Vacuum/Strength And Toughness Die Casting Technology

High Vacuum/Strength And Toughness Die Casting Technology

High vacuum die-casting technology refers to the liquid metal filling the mold cavity at a very high speed under the action of high pressure, and the liquid metal is cooled and solidified through a certain pressure, so as to obtain die-cast castings. Starting from the current status of the developme ...

How To Calculate The Price Of Die Casting Parts And Molds

How To Calculate The Price Of Die Casting Parts And Molds

There are many ways to settle the mold, and they are not the same. But they all have one thing in common, that is, efforts to organically combine the technical and economic indicators of the mold to produce mutual benefits for both parties. Make the mold from the evaluation to the quotation, from th ...

The Difference Between Aluminum Die Casting And Gravity Casting

The Difference Between Aluminum Die Casting And Gravity Casting

Aluminum alloy is widely used in automobile manufacturing, aerospace, shipbuilding and other fields because of its good plasticity, corrosion resistance, and light weight. With the development of China's manufacturing industry, the demand for aluminum alloy and aluminum alloy castings is increasing, ...

The Most Complete Standards For Molds Acceptance

The Most Complete Standards For Molds Acceptance

Generally, the length of circular perforation weld mark is not more than 5mm, and the length of special-shaped perforation weld mark is less than 15mm, and the weld mark strength can pass the functional safety test. ...

The Expanding Application Field Of Aluminum Alloy Die Casting

The Expanding Application Field Of Aluminum Alloy Die Casting

Since the 1990s, China's die-casting industry has achieved amazing development and has developed into a new industry. At present, the aluminum alloy die-casting process has become one of the most widely used processes in the automotive aluminum alloy forming process, accounting for 49% of the variou ...

MingHe Casting Advantage

  • Comprehensive Casting design software and skilled engineer enables sample to be done within 15-25 days
  • Complete set of inspection equipment & quality control makes excellent Die Casting products
  • A fine shipping process and good supplier guarantee we can always deliver Die Casting goods on time
  • From prototypes to end parts, upload your CAD files, fast and professional quote in 1-24 hours
  • Wide-ranging capabilities for designing prototypes or massive manufacturing end use Die Casting parts
  • Advanced Die Casting techniques (180-3000T Machine,Cnc Machining, CMM) process a variety of metal & plastic materials

HelpFul Articles

How To Calculate Pressure Die Casting Tonnage

Calculation Formula The calculation formula for the selection of die-casting machine: Die-casting m

How To Find The Best Position Of Vacuum Valve In The Die Cast Tooling?

Compared with sand casting and gravity casting, the microstructure of traditional die castings is no

The Key Points Of Aluminum Alloy Die Casting Design

An excellent die casting designer should be familiar with the die casting process and the production

The Comprehensive Diagnosis And Control Of Automobile Aluminum Die Castings Quality

With the continuous development of sports and science and technology, people's living standards cont

The Solutions And Preventive Measures For Aluminum Die Casting 10 Major Defects

There are stripes on the surface of the casting that are consistent with the flow direction of the m

High Vacuum/Strength And Toughness Die Casting Technology

High vacuum die-casting technology refers to the liquid metal filling the mold cavity at a very high