The life of the continuous casting tundish determines the index of the number of continuous casting furnaces in a single ladle, and the life of the tundish is unstable, which will directly affect the production, resulting in an increase in the cost of the production process.

The Measures To Improve Continuous Casting Tundish Life

Factors affecting the life of the continuous casting tundish: severe erosion of the working layer in the impact zone during the pouring process, floating of the impact plate, expansion of the working layer, and material collapse. These restrict the improvement of the life of the tundish and become a restrictive link in the production stability of steel mills. The measures to be taken are:

1. Dry material

Analyze the physical and chemical indexes of each batch of dry materials, and check the actual comparison at the same time, take the content of magnesium oxide in the dry materials and the magnesia particle size and crystallinity as the preliminary judgment of the quality of each batch of dry materials, and then combine the trial The effect determines its planned service life, avoiding unreasonable aggregate ratio and reducing the strength of the working layer.

2. Angle of large package casing

In the installation of the long casing of the large package, the inclination angle of the casing is artificially controlled, and the vortex of the flow field in the impact area can be moved to the middle area of ​​the tundish by taking the slope of 5-10° to the opposite direction of the outer wall of the impact area as a reference. , To avoid erosion.

3. The length and depth of the tundish

According to the actual situation of the casting machine, by adjusting the length of the long sleeve of the tundish to reasonably control the depth of the sleeve immersion into the tundish liquid level, it is advisable that the liquid level of the tundish does not fluctuate drastically, and the immersion depth should be referred to 200-300mm to avoid erosion.

4. Impact plate seams

Control the viscosity of the joint material of the impact plate. After the two impact plates are overlapped, the upper impact plate can be rotated 360° to achieve uniform joint material at the joint of the impact plate to avoid gaps between the two impact plates. .

5. Dry material around the impact plate

After the impact plate is installed, the dry material around the impact plate can be filled manually with special tools, which can avoid the weakening of the strength due to the blind zone of vibration in this area; in addition, before vibration, control the dry material around the impact plate. The type material is higher than the height of the impact plate, and the bottom of the impact area is designed to be concave, which can enhance the vibration effect of the dry material at the bottom of the impact area, and to a certain extent can prevent the impact plate from floating during the pouring process.

6. Baking process

According to the actual production of the steel plant, the baking process that meets its own conditions is formulated. When conditions permit, it is possible to appropriately extend the baking time at low and medium heat to improve the baking quality of the tundish and avoid the expansion or collapse of the working layer after the tundish is baked.


Please keep the source and address of this article for reprinting:The Measures To Improve Continuous Casting Tundish Life  


Minghe Casting Company are dedicated to manufacture and provide quality and high performance Casting Parts(metal die casting parts range mainly include Thin-Wall Die Casting,Hot Chamber Die Casting,Cold Chamber Die Casting),Round Service(Die Casting Service,Cnc Machining,Mold Making,Surface Treatment).Any custom Aluminum die casting, magnesium or Zamak/zinc die casting and other castings requirements are welcome to contact us.

ISO90012015 AND ITAF 16949 CASTING COMPANY SHOP

Under the control of ISO9001 and TS 16949,All processes are carried out through hundreds of advanced die casting machines, 5-axis machines, and other facilities, ranging from blasters to Ultra Sonic washing machines.Minghe not only has advanced equipment but also have professional team of experienced engineers,operators and inspectors to make the customer’s design come true.

POWERFUL ALUMINUM DIE CASTING WITH ISO90012015

Contract manufacturer of die castings. Capabilities include cold chamber aluminum die casting parts from 0.15 lbs. to 6 lbs., quick change set up, and machining. Value-added services include polishing, vibrating, deburring, shot blasting, painting, plating, coating, assembly, and tooling. Materials worked with include alloys such as 360, 380, 383, and 413.

PERFECT ZINC DIE CASTING PARTS IN CHINA

Zinc die casting design assistance/concurrent engineering services. Custom manufacturer of precision zinc die castings. Miniature castings, high pressure die castings, multi-slide mold castings, conventional mold castings, unit die and independent die castings and cavity sealed castings can be manufactured. Castings can be manufactured in lengths and widths up to 24 in. in +/-0.0005 in. tolerance.  

ISO 9001 2015 certified manufacturer of die cast magnesium and mold manufacturing

ISO 9001: 2015 certified manufacturer of die cast magnesium, Capabilities include high-pressure magnesium die casting up to 200 ton hot chamber & 3000 ton cold chamber, tooling design, polishing, molding, machining, powder & liquid painting, full QA with CMM capabilities, assembly, packaging & delivery.

Minghe Casting Additional Casting Service-investment casting etc

ITAF16949 certified. Additional Casting Service Include investment casting,sand casting,Gravity Casting, Lost Foam Casting,Centrifugal Casting,Vacuum Casting,Permanent Mold Casting,.Capabilities include EDI, engineering assistance, solid modeling and secondary processing.

Casting Parts Application Case Studies

Casting Industries Parts Case Studies for: Cars, Bikes, Aircraft, Musical instruments, Watercraft, Optical devices, Sensors, Models, Electronic devices, Enclosures, Clocks, Machinery, Engines, Furniture, Jewelry, Jigs, Telecom, Lighting, Medical devices, Photographic devices, Robots, Sculptures, Sound equipment, Sporting equipment, Tooling, Toys and more. 


What Can we help you do next?

∇ Go To Homepage For Die Casting China

→Casting Parts-Find out what we have done.

→Ralated Tips About Die Casting Services


By Minghe Die Casting Manufacturer |Categories: Helpful Articles |Material Tags: , , , , , ,Bronze Casting,Casting Video,Company History,Aluminum Die Casting |Comments Off

MingHe Casting Advantage

  • Comprehensive Casting design software and skilled engineer enables sample to be done within 15-25 days
  • Complete set of inspection equipment & quality control makes excellent Die Casting products
  • A fine shipping process and good supplier guarantee we can always deliver Die Casting goods on time
  • From prototypes to end parts, upload your CAD files, fast and professional quote in 1-24 hours
  • Wide-ranging capabilities for designing prototypes or massive manufacturing end use Die Casting parts
  • Advanced Die Casting techniques (180-3000T Machine,Cnc Machining, CMM) process a variety of metal & plastic materials

HelpFul Articles

The Measures To Improve Continuous Casting Tundish Life

The life of the continuous casting tundish determines the index of the number of continuous casting

The Measures To Improve The Life Of Aluminum-Magnesium Alloy Die Casting Mold

As an important processing equipment, aluminum-magnesium alloy die-casting molds have a direct impac

5 Major Links Need To Be Controlled To Improve Mold Life

Including mold production plan formulation, mold design, process formulation, workshop task assignme

How to improve the service life of the intermediate frequency furnace?

Improving the service life of the induction furnace body is the goal pursued by every foundry worker

The Measures To Improve High Anti-Collapse Casing Life

The problem of casing damage seriously restricts oil and gas production, reduces the production life

The Factors Influencing The Fatigue Life Of Rolling Bearings

In recent years, the tribological design of general mechanical parts has received widespread attenti