How Does Silicon Carbide Improve The Quality Of Castings?
The addition of silicon carbide can prevent the precipitation of carbides, increase the amount of ferrite, make the cast iron structure dense, significantly improve the processing performance and make the cutting surface smooth. Increase the number of graphite balls per unit area of nodular cast i ...