High wear-resistant cold work die steel is generally high carbon high chromium steel, representative steel grades are: Cr12, Cr12MoV, Cr12Mo1V1, Cr12W, Cr12V, LD (7Cr7Mo2V2Si), ER5 (Cr8MoWV3Si), GM (9Cr6-W3Mo2V2) and so on.

Most of the above steels are ledeburite steels. There are a large number of eutectic carbides in the structure. There are a large number of eutectic carbides after vacuum quenching. The wear resistance is high and the bearing capacity is large. It is often used for manufacturing under high wear resistance conditions. Die for cold working of work.

High Wear-Resistant Cold Work Die Steel Heat Treatment Process

The correct selection of the heat treatment of the material is the key to the manufacture of the bearing. I have done the vacuum low-quenching and low-return process and heat treatment distortion statistics for the bearing bush working in the polyvinyl alcohol (PVA) slurry. In this article, the bearing bush is working in the polyester (PET) slurry, and the use temperature is higher, at 350 ℃ About, higher than the use temperature of PVA slurry (about 100℃), the bearing is planned to adopt high quenching and high heat treatment process.

The processing procedures of the bearing bush are blanking→forging→spheroidizing annealing→machining→vacuum quenching and tempering→grinding, etc. This experiment observes and tests the microstructure, hardness and heat treatment distortion of the bearing bush after the spheroidizing annealing and high quenching and high recovery process, so as to provide future process adjustments for this type of material and the size processing allowance before quenching. reference.

At present, the heat treatment of Cr12 materials accounts for more than 50% of the processing capacity of cold work molds. Mastering the different heat treatment processes, microstructure characteristics and distortion laws of these materials has positive guiding significance for the manufacture of molds in scientific research and production.

Cr12MoV steel bearing bush is a kind of bearing part used in chemical, machinery and other industries. It works under specific pressure, temperature and medium. The operating conditions are harsh and the manufacturing process is complex. In addition to maintaining high hardness under certain temperature conditions, the Cr12MoV steel for the manufacture of bearing bushes must also have wear resistance, corrosion resistance, oxidation resistance, good dimensional stability and good quilting. Processing performance, etc.


Please keep the source and address of this article for reprinting: High Wear-Resistant Cold Work Die Steel Heat Treatment Process


Minghe Die Casting Company are dedicated to manufacture and provide quality and high performance Casting Parts(metal die casting parts range mainly include Thin-Wall Die Casting,Hot Chamber Die Casting,Cold Chamber Die Casting),Round Service(Die Casting Service,Cnc Machining,Mold Making,Surface Treatment).Any custom Aluminum die casting, magnesium or Zamak/zinc die casting and other castings requirements are welcome to contact us.

ISO90012015 AND ITAF 16949 CASTING COMPANY SHOP

Under the control of ISO9001 and TS 16949,All processes are carried out through hundreds of advanced die casting machines, 5-axis machines, and other facilities, ranging from blasters to Ultra Sonic washing machines.Minghe not only has advanced equipment but also have professional team of experienced engineers,operators and inspectors to make the customer’s design come true.

POWERFUL ALUMINUM DIE CASTING WITH ISO90012015

Contract manufacturer of die castings. Capabilities include cold chamber aluminum die casting parts from 0.15 lbs. to 6 lbs., quick change set up, and machining. Value-added services include polishing, vibrating, deburring, shot blasting, painting, plating, coating, assembly, and tooling. Materials worked with include alloys such as 360, 380, 383, and 413.

PERFECT ZINC DIE CASTING PARTS IN CHINA

Zinc die casting design assistance/concurrent engineering services. Custom manufacturer of precision zinc die castings. Miniature castings, high pressure die castings, multi-slide mold castings, conventional mold castings, unit die and independent die castings and cavity sealed castings can be manufactured. Castings can be manufactured in lengths and widths up to 24 in. in +/-0.0005 in. tolerance.  

ISO 9001 2015 certified manufacturer of die cast magnesium and mold manufacturing

ISO 9001: 2015 certified manufacturer of die cast magnesium, Capabilities include high-pressure magnesium die casting up to 200 ton hot chamber & 3000 ton cold chamber, tooling design, polishing, molding, machining, powder & liquid painting, full QA with CMM capabilities, assembly, packaging & delivery.

Minghe Casting Additional Casting Service-investment casting etc

ITAF16949 certified. Additional Casting Service Include investment casting,sand casting,Gravity Casting, Lost Foam Casting,Centrifugal Casting,Vacuum Casting,Permanent Mold Casting,.Capabilities include EDI, engineering assistance, solid modeling and secondary processing.

Casting Parts Application Case Studies

Casting Industries Parts Case Studies for: Cars, Bikes, Aircraft, Musical instruments, Watercraft, Optical devices, Sensors, Models, Electronic devices, Enclosures, Clocks, Machinery, Engines, Furniture, Jewelry, Jigs, Telecom, Lighting, Medical devices, Photographic devices, Robots, Sculptures, Sound equipment, Sporting equipment, Tooling, Toys and more. 


What Can we help you do next?

∇ Go To Homepage For Die Casting China

→Casting Parts-Find out what we have done.

→Ralated Tips About Die Casting Services


By Minghe Die Casting Manufacturer |Categories: Helpful Articles |Material Tags: , , , , , ,Bronze Casting,Casting Video,Company History,Aluminum Die Casting |Comments Off

MingHe Casting Advantage

  • Comprehensive Casting design software and skilled engineer enables sample to be done within 15-25 days
  • Complete set of inspection equipment & quality control makes excellent Die Casting products
  • A fine shipping process and good supplier guarantee we can always deliver Die Casting goods on time
  • From prototypes to end parts, upload your CAD files, fast and professional quote in 1-24 hours
  • Wide-ranging capabilities for designing prototypes or massive manufacturing end use Die Casting parts
  • Advanced Die Casting techniques (180-3000T Machine,Cnc Machining, CMM) process a variety of metal & plastic materials

HelpFul Articles

High Vacuum/Strength And Toughness Die Casting Technology

High vacuum die-casting technology refers to the liquid metal filling the mold cavity at a very high

Research Trends Of Heat Treatment Of High-Strength Steel, DP Steel And Martensitic Steel

With the increase in strength of steel materials, martensite is used in various steels. However, bec

Influence of High Temperature Nitrogen Solution Treatment on Corrosion Resistance

Nitriding and carburizing treatment on the surface of steel products can improve the mechanical prop

The Influencing Factors Of 500MPa Grade V-N Microalloyed High-strength Steel Bars Properties

The effect of nitrogen content on the mechanical properties of 500MPa grade VN microalloyed high-str

The Role Of Various Elements In High-Strength Martensitic Wear-Resistant Steel

About 80% of the failures of mechanical parts are caused or induced by various forms of wear. Abrasi

Effect of homogenization treatment on high temperature deformation characteristics of as cast Incoloy800 alloy

Incoloy800 is a solid solution reinforced austenite alloy, which has high creep fracture strength, g

The Heat Treatment Process Of High Manganese And Low Nickel Stainless Steel

In recent years, with the rapid development of China's economy, the demand for stainless steel has c

The Measures To Improve High Anti-Collapse Casing Life

The problem of casing damage seriously restricts oil and gas production, reduces the production life

The Optimization Of Low-Alloy High-Strength Steel Welding Consumables Composition

The optimization direction of the weld structure of low-alloy high-strength steel is to generate mor

High Pressure Forming Process In Support Pressure

Internal high pressure forming is also called hydroforming or hydraulic forming. It is a material fo

High Ammonia Nitrogen Wastewater Treatment Technology For Tungsten And Molybdenum Smelting

Tungsten and cobalt are important additive elements for high-performance steel, but a large amount o

Research On New Forged High Speed Steel Roll Material Quenching Process

Modern large-scale cold strip rolling mills have realized headless and semi-endless rolling. The req

Easy To Weld Ultra High Strength Steel For The Coal Industry

A few days ago, the first batch of 1,200-ton contract for the easy-weld ultra-high-strength steel Q8

The Properties Of Pyrowear 53 High-Strength Alloy Steel

Compared with other high-strength alloy steels with similar chemical composition and processing tech