Effect of homogenization treatment on high temperature deformation characteristics of as cast Incoloy800 alloy

Publish Time: Author: Site Editor Visit: 33758

Incoloy800 is a solid solution reinforced austenite alloy, which has high creep fracture strength, good high temperature mechanical properties and corrosion resistance. It is widely used in nuclear power, petrochemical and other key parts. In order to meet the needs of industrial production, most of the as cast austenite alloys need to be obtained by hot rolling, hot forging and other hot-processing processes. In the process of hot deformation, the alloy is prone to surface defects and even cracks. In engineering, the defects are usually prevented by adjusting the heating temperature and holding time before the thermal deformation. From the production experience, the heating temperature and the holding time have a great influence on the crack.

Effect of homogenization treatment on high temperature deformation characteristics of as cast Incoloy800 alloy

The previous research focuses on the effect of homogenization on the structure and the second phase, and the effect of homogenization on the mechanical properties of materials needs further understanding. The researchers studied the effect of homogenization on the deformation properties of 800 alloy by high temperature compression experiment.

It is melted by vacuum induction furnace and produced by pouring Φ 80mm × The chemical composition (mass fraction,%) of the 300 mm Incoloy800 ingot is fe41.2, ni31.5, cr21.1, mn1.30, c0.06, ti0.3, al0.26, cu0.60, si0.95. To intercept on ingots Φ 8mm × The height of the sample is parallel to the diameter of the ingot, and a part of the specimens treated by homogenization are subjected to thermal compression test. The homogenization treatment specification is 1250 ℃ for 2 hours, and then cooled with the furnace.

The uniaxial thermal compression test was carried out on the original sample and the homogenized sample on thermorester-w thermal / force simulation test machine, and glass powder was used as lubricant. The deformation temperature is 950-1200 ℃, the temperature interval is 50 ℃, the sample is heated to the preset deformation temperature at 10 ℃ /s, and the temperature is kept for 120s, and then the deformation is carried out at the strain rate of 0.1s-1, with the maximum true strain of 0.5. After the thermal deformation, the deformed sample was cut symmetrically along the axial direction by wire cutting method. The microstructure of the metallographic sample was observed after corrosion. The test results are as follows:

  • (1) The yield stress of 800 alloy was reduced by homogenization treatment at 1250 ℃ for 2 hours, and the decrease of the deformation temperature gradually decreased.
  • (2) No recrystallization occurred in the high temperature deformation samples, and homogenization treatment had no effect on the high temperature rheological process.
  • (3) The morphology of carbide at the grain boundary of 800 alloy was changed by homogenization treatment, and the carbide changed from compact layer to discontinuous particle. Compared with lamellar carbides, granular carbide leads to low density dislocation during high temperature deformation, which reduces the deformation resistance and decreases the yield strength at high temperature.

Please keep the source and address of this article for reprinting:Effect of homogenization treatment on high temperature deformation characteristics of as cast Incoloy800 alloy


Minghe Die Casting Company are dedicated to manufacture and provide quality and high performance Casting Parts(metal die casting parts range mainly include Thin-Wall Die Casting,Hot Chamber Die Casting,Cold Chamber Die Casting),Round Service(Die Casting Service,Cnc Machining,Mold Making,Surface Treatment).Any custom Aluminum die casting, magnesium or Zamak/zinc die casting and other castings requirements are welcome to contact us.

ISO90012015 AND ITAF 16949 CASTING COMPANY SHOP

Under the control of ISO9001 and TS 16949,All processes are carried out through hundreds of advanced die casting machines, 5-axis machines, and other facilities, ranging from blasters to Ultra Sonic washing machines.Minghe not only has advanced equipment but also have professional team of experienced engineers,operators and inspectors to make the customer’s design come true.

POWERFUL ALUMINUM DIE CASTING WITH ISO90012015

Contract manufacturer of die castings. Capabilities include cold chamber aluminum die casting parts from 0.15 lbs. to 6 lbs., quick change set up, and machining. Value-added services include polishing, vibrating, deburring, shot blasting, painting, plating, coating, assembly, and tooling. Materials worked with include alloys such as 360, 380, 383, and 413.

PERFECT ZINC DIE CASTING PARTS IN CHINA

Zinc die casting design assistance/concurrent engineering services. Custom manufacturer of precision zinc die castings. Miniature castings, high pressure die castings, multi-slide mold castings, conventional mold castings, unit die and independent die castings and cavity sealed castings can be manufactured. Castings can be manufactured in lengths and widths up to 24 in. in +/-0.0005 in. tolerance.  

ISO 9001 2015 certified manufacturer of die cast magnesium and mold manufacturing

ISO 9001: 2015 certified manufacturer of die cast magnesium, Capabilities include high-pressure magnesium die casting up to 200 ton hot chamber & 3000 ton cold chamber, tooling design, polishing, molding, machining, powder & liquid painting, full QA with CMM capabilities, assembly, packaging & delivery.

Minghe Casting Additional Casting Service-investment casting etc

ITAF16949 certified. Additional Casting Service Include investment casting,sand casting,Gravity Casting, Lost Foam Casting,Centrifugal Casting,Vacuum Casting,Permanent Mold Casting,.Capabilities include EDI, engineering assistance, solid modeling and secondary processing.

Casting Parts Application Case Studies

Casting Industries Parts Case Studies for: Cars, Bikes, Aircraft, Musical instruments, Watercraft, Optical devices, Sensors, Models, Electronic devices, Enclosures, Clocks, Machinery, Engines, Furniture, Jewelry, Jigs, Telecom, Lighting, Medical devices, Photographic devices, Robots, Sculptures, Sound equipment, Sporting equipment, Tooling, Toys and more. 


What Can we help you do next?

∇ Go To Homepage For Die Casting China

→Casting Parts-Find out what we have done.

→Ralated Tips About Die Casting Services


By Minghe Die Casting Manufacturer |Categories: Helpful Articles |Material Tags: , , , , , ,Bronze Casting,Casting Video,Company History,Aluminum Die Casting |Comments Off

MingHe Casting Advantage

  • Comprehensive Casting design software and skilled engineer enables sample to be done within 15-25 days
  • Complete set of inspection equipment & quality control makes excellent Die Casting products
  • A fine shipping process and good supplier guarantee we can always deliver Die Casting goods on time
  • From prototypes to end parts, upload your CAD files, fast and professional quote in 1-24 hours
  • Wide-ranging capabilities for designing prototypes or massive manufacturing end use Die Casting parts
  • Advanced Die Casting techniques (180-3000T Machine,Cnc Machining, CMM) process a variety of metal & plastic materials

HelpFul Articles

Realize High-Speed Steel Induction Heating And Quenching

The heating speed of induction heating ranges from tens of degrees per second to hundreds of degrees

The Combination Of Powder Coating For Foundry And High-Efficiency Flow Coating Process

Casting coatings are applied to most of the casting production process and play an important role in

The Forming Technology Of High-Strength Steel For Automobiles

Automobiles use high-strength steel, which can reduce the thickness of the plate due to its higher s

The Composition Of High Vacuum Magnetic Field Heat Treatment Device

Magnetic field heat treatment has attracted much attention in the field of materials research becaus

The Effect of Solution Treatment On G80T High Temperature Bearing Steel

G80T steel is a special type of M50 steel smelted by electroslag directional solidification, which b

High-Strength Gray Cast Iron Smelting Technology

This article introduces how to obtain high-strength gray cast iron smelting technology under the con

High Wear-Resistant Cold Work Die Steel Heat Treatment Process

High wear-resistant cold work die steel is generally high carbon high chromium steel, representative

How To Make Higher Value For Die Casting Mold Application

The mold design manual has detailed the problems that should be paid attention to in the design of t

Decrypt The Reason For High Temperature Hydraulic Oil System

Excessive temperature rise of hydraulic oil can cause thermal deformation of the machine. Moving par

The Measures And Effects Of Nitrogen Increase In High Nitrogen Stainless Steel Melting

High-nitrogen stainless steel refers to a steel with a ferrite matrix with a nitrogen content of mor

High Pressure Forming Process In Support Pressure

Internal high pressure forming is also called hydroforming or hydraulic forming. It is a material fo

High Ammonia Nitrogen Wastewater Treatment Technology For Tungsten And Molybdenum Smelting

Tungsten and cobalt are important additive elements for high-performance steel, but a large amount o

Research On New Forged High Speed Steel Roll Material Quenching Process

Modern large-scale cold strip rolling mills have realized headless and semi-endless rolling. The req

Easy To Weld Ultra High Strength Steel For The Coal Industry

A few days ago, the first batch of 1,200-ton contract for the easy-weld ultra-high-strength steel Q8

The Properties Of Pyrowear 53 High-Strength Alloy Steel

Compared with other high-strength alloy steels with similar chemical composition and processing tech