Research Trends Of Heat Treatment Of High-Strength Steel, DP Steel And Martensitic Steel

Publish Time: Author: Site Editor Visit: 32752

With the increase in strength of steel materials, martensite is used in various steels. However, because the martensite structure is fine and complex, and the strengthening mechanism is not simple, it is very complicated to find out the mechanism to increase the strength. In addition, there are original austenite grains, flaky structure and lath structure in martensite, and there are still many unclear points about their influence on the mechanical properties of steel. Therefore, some research reports have used the nano-molding method to measure the hardness in the martensite, and studied the influence of the martensite structure on the hardness of the steel.

Research trends of heat treatment of high-strength steel, DP steel and martensitic steel

The matrix structure is martensite, and the TRIP martensitic steel (TM steel) that effectively utilizes the martensite-austenite mixed phase (MA phase) is expected to become 1.5MPa for cold stamping and hot stamping of car parts Grade ultra-high-strength steel plate. Previous research reports pointed out that the retained austenite (R) characteristics of TM steel will vary greatly due to the difference in cooling rate after austenitization. There are research reports on the influence of the cooling rate after austenitization on the tensile properties and impact toughness of TM steel.

Ultra-high-strength TRIP-type martensitic steel (TM steel) with a matrix of lath martensite structure has ultra-high strength and good stretch flangeability, so it is expected to become a new generation of high-strength steel plates for automobiles. The TM steel is produced by performing isothermal transformation treatment (IT treatment) below the martensitic transformation end temperature (Mf), but there are few research reports on the influence of IT treatment temperature on formability. The research report investigated the influence of IT treatment temperature on the tensile properties and formability of TM steel sheets. In addition, there are research reports on the relationship between the formability of the TM steel sheet, the fine structure and the metallic structure such as the characteristics of retained austenite (R).

The tensile properties of DP steel are greatly affected by the hardness and volume ratio of martensite (hereinafter referred to as "M") as a strengthened structure. Moreover, it is well known that the ductile fracture behavior of DP steel is closely related to M. However, with regard to changes in the composition of the steel sheet and heat treatment conditions, not only the hardness of M will change, but also the volume fraction and shape of M will also change at the same time. Therefore, it is difficult to simply evaluate the effect of M hardness on ductile fracture behavior. Evaluation. A research report investigated the influence of M hardness on the tensile properties and hollow formation of DP steel with tempering control hardness.


Please keep the source and address of this article for reprinting: Research trends of heat treatment of high-strength steel, DP steel and martensitic steel


Minghe Die Casting Company are dedicated to manufacture and provide quality and high performance Casting Parts(metal die casting parts range mainly include Thin-Wall Die Casting,Hot Chamber Die Casting,Cold Chamber Die Casting),Round Service(Die Casting Service,Cnc Machining,Mold Making,Surface Treatment).Any custom Aluminum die casting, magnesium or Zamak/zinc die casting and other castings requirements are welcome to contact us.

ISO90012015 AND ITAF 16949 CASTING COMPANY SHOP

Under the control of ISO9001 and TS 16949,All processes are carried out through hundreds of advanced die casting machines, 5-axis machines, and other facilities, ranging from blasters to Ultra Sonic washing machines.Minghe not only has advanced equipment but also have professional team of experienced engineers,operators and inspectors to make the customer’s design come true.

POWERFUL ALUMINUM DIE CASTING WITH ISO90012015

Contract manufacturer of die castings. Capabilities include cold chamber aluminum die casting parts from 0.15 lbs. to 6 lbs., quick change set up, and machining. Value-added services include polishing, vibrating, deburring, shot blasting, painting, plating, coating, assembly, and tooling. Materials worked with include alloys such as 360, 380, 383, and 413.

PERFECT ZINC DIE CASTING PARTS IN CHINA

Zinc die casting design assistance/concurrent engineering services. Custom manufacturer of precision zinc die castings. Miniature castings, high pressure die castings, multi-slide mold castings, conventional mold castings, unit die and independent die castings and cavity sealed castings can be manufactured. Castings can be manufactured in lengths and widths up to 24 in. in +/-0.0005 in. tolerance.  

ISO 9001 2015 certified manufacturer of die cast magnesium and mold manufacturing

ISO 9001: 2015 certified manufacturer of die cast magnesium, Capabilities include high-pressure magnesium die casting up to 200 ton hot chamber & 3000 ton cold chamber, tooling design, polishing, molding, machining, powder & liquid painting, full QA with CMM capabilities, assembly, packaging & delivery.

Minghe Casting Additional Casting Service-investment casting etc

ITAF16949 certified. Additional Casting Service Include investment casting,sand casting,Gravity Casting, Lost Foam Casting,Centrifugal Casting,Vacuum Casting,Permanent Mold Casting,.Capabilities include EDI, engineering assistance, solid modeling and secondary processing.

Casting Parts Application Case Studies

Casting Industries Parts Case Studies for: Cars, Bikes, Aircraft, Musical instruments, Watercraft, Optical devices, Sensors, Models, Electronic devices, Enclosures, Clocks, Machinery, Engines, Furniture, Jewelry, Jigs, Telecom, Lighting, Medical devices, Photographic devices, Robots, Sculptures, Sound equipment, Sporting equipment, Tooling, Toys and more. 


What Can we help you do next?

∇ Go To Homepage For Die Casting China

→Casting Parts-Find out what we have done.

→Ralated Tips About Die Casting Services


By Minghe Die Casting Manufacturer |Categories: Helpful Articles |Material Tags: , , , , , ,Bronze Casting,Casting Video,Company History,Aluminum Die Casting |Comments Off

MingHe Casting Advantage

  • Comprehensive Casting design software and skilled engineer enables sample to be done within 15-25 days
  • Complete set of inspection equipment & quality control makes excellent Die Casting products
  • A fine shipping process and good supplier guarantee we can always deliver Die Casting goods on time
  • From prototypes to end parts, upload your CAD files, fast and professional quote in 1-24 hours
  • Wide-ranging capabilities for designing prototypes or massive manufacturing end use Die Casting parts
  • Advanced Die Casting techniques (180-3000T Machine,Cnc Machining, CMM) process a variety of metal & plastic materials

HelpFul Articles

Research on the influence of hydrogen on the strength of steel

As we all know, the hydrogen in the material will be trapped at various trap positions (dislocations

Research On Die Casting Mould Gating System

Die casting is one of the important means for non-ferrous metal forming. During the die-casting proc

Research on Entrainment Behavior of Aluminum Alloy Castings in Low Pressure Die Casting Process Based on Flow-3D

Based on Flow-3D software, the filling process of low pressure casting of three different structures

Research on Structure and Performance of Low Pressure Casting Aluminum Alloy Rear Sub-frame

As the world pays more and more attention to the problem of environmental pollution, automobile comp

Research Trends Of Heat Treatment Of High-Strength Steel, DP Steel And Martensitic Steel

With the increase in strength of steel materials, martensite is used in various steels. However, bec

Research Trends In Heat Treatment Of Heat Resistant Alloys And Superalloys

One of the most important issues for the development of 700 ℃ steam temperature A-USC generator sets

Research And Development Of Medical Stainless Steel In China

Stainless steel is a kind of special steel material. The Cr content in the steel must exceed 12% to

The Process Application And Research of Resin Sand Casting Method

Compared with the clay sand dry casting process, the self-hardening resin sand casting process has t

The Research On Joint Welds Of NiCrMoV Dissimilar Steel Properties And Microstructure

The rotor is one of the core components of large steam turbine equipment. At present, there are main

The Research And Application Of Smelting Non-Fluoride Slagging

Fluorite is used as a slag-making agent in the steelmaking process. The calcium fluoride in the conv