According to the American AISI standard, stainless steel is represented by three-digit Arabic numerals. The first digit indicates the category, and the second and third digits indicate the sequence number. The 300 series stainless steel whose first digit starts with 3 is austenitic stainless steel with a Cr-Ni structure. Common grades are:

1.304 low-carbon austenitic stainless and acid-resistant steel

Performance: general resistance to intergranular corrosion and excellent corrosion resistance, and has a certain degree of corrosion resistance to alkalis and most organic and inorganic acids. Uses: Widely used in decoration and acid pipelines, chemical equipment, etc. The Guangdong Stainless Steel Materials and Products Association has some pipe-making member companies that produce 304 stainless steel decorative pipes, product pipes and decorative panels.

2.304L low carbon austenitic stainless steel

Performance: It has good resistance to crystal and corrosion, and has good corrosion resistance in various strong corrosive media. Uses: Suitable for petrochemical corrosion-resistant equipment parts, especially welded pipe fittings that cannot be heat-treated after welding.

3.304H austenitic stainless heat-resistant steel

Performance: good corrosion resistance and welding performance, good thermal strength. Uses: Mainly used in large boiler superheaters, reheaters, steam pipes, and petrochemical heat exchangers.

4.316 austenitic stainless hot-strength steel

Performance: Good corrosion resistance and pitting resistance to a variety of inorganic acids, organic acids, alkalis, and salts, and good variable strength at high temperatures. Uses: Suitable for large-scale boiler superheaters, reheaters, steam pipes, petrochemical heat exchanger pipe fittings, and can be used as pitting corrosion resistant materials.

5.316L ultra-low carbon austenitic stainless steel

Performance: It has good resistance to crystal and corrosion, and has good corrosion resistance to organic acids, alkalis and salts. Uses: Widely used in acid pipelines and chemical equipment, etc.

6.321 austenitic stainless acid-resistant steel

Performance: It has high resistance to intergranular corrosion, and has good corrosion resistance to some organic and inorganic acids. Uses: used in the manufacture of acid-resistant transportation pipelines, large boiler superheaters, reheaters, steam pipelines, petrochemical heat exchangers, etc.

7.317L austenitic stainless acid-resistant steel

Performance: Excellent corrosion resistance, better resistance to pitting corrosion in chloride-containing solutions. Uses: To manufacture main resistant pipes for industrial equipment such as synthetic fiber, petrochemical, textile, papermaking and atomic energy post-processing.

8.310S austenitic heat-resistant stainless steel

Performance: Good resistance to intergranular corrosion, excellent resistance to chloride stress corrosion, and good resistance to high temperature oxidation. Uses: used to make furnace tubes, boiler superheaters, heat exchanger pipe fittings.

9.347H austenitic stainless hot-strength steel

Performance: It has good corrosion resistance, welding performance and thermal strength. Uses: used in large boiler superheaters, reheaters, steam pipes, and petrochemical heat exchanger pipe fittings.


Please keep the source and address of this article for reprinting: The Performance Of 300 Series Stainless Steel


Minghe Die Casting Company are dedicated to manufacture and provide quality and high performance Casting Parts(metal die casting parts range mainly include Thin-Wall Die Casting,Hot Chamber Die Casting,Cold Chamber Die Casting),Round Service(Die Casting Service,Cnc Machining,Mold Making,Surface Treatment).Any custom Aluminum die casting, magnesium or Zamak/zinc die casting and other castings requirements are welcome to contact us.

ISO90012015 AND ITAF 16949 CASTING COMPANY SHOP

Under the control of ISO9001 and TS 16949,All processes are carried out through hundreds of advanced die casting machines, 5-axis machines, and other facilities, ranging from blasters to Ultra Sonic washing machines.Minghe not only has advanced equipment but also have professional team of experienced engineers,operators and inspectors to make the customer’s design come true.

POWERFUL ALUMINUM DIE CASTING WITH ISO90012015

Contract manufacturer of die castings. Capabilities include cold chamber aluminum die casting parts from 0.15 lbs. to 6 lbs., quick change set up, and machining. Value-added services include polishing, vibrating, deburring, shot blasting, painting, plating, coating, assembly, and tooling. Materials worked with include alloys such as 360, 380, 383, and 413.

PERFECT ZINC DIE CASTING PARTS IN CHINA

Zinc die casting design assistance/concurrent engineering services. Custom manufacturer of precision zinc die castings. Miniature castings, high pressure die castings, multi-slide mold castings, conventional mold castings, unit die and independent die castings and cavity sealed castings can be manufactured. Castings can be manufactured in lengths and widths up to 24 in. in +/-0.0005 in. tolerance.  

ISO 9001 2015 certified manufacturer of die cast magnesium and mold manufacturing

ISO 9001: 2015 certified manufacturer of die cast magnesium, Capabilities include high-pressure magnesium die casting up to 200 ton hot chamber & 3000 ton cold chamber, tooling design, polishing, molding, machining, powder & liquid painting, full QA with CMM capabilities, assembly, packaging & delivery.

Minghe Casting Additional Casting Service-investment casting etc

ITAF16949 certified. Additional Casting Service Include investment casting,sand casting,Gravity Casting, Lost Foam Casting,Centrifugal Casting,Vacuum Casting,Permanent Mold Casting,.Capabilities include EDI, engineering assistance, solid modeling and secondary processing.

Casting Parts Application Case Studies

Casting Industries Parts Case Studies for: Cars, Bikes, Aircraft, Musical instruments, Watercraft, Optical devices, Sensors, Models, Electronic devices, Enclosures, Clocks, Machinery, Engines, Furniture, Jewelry, Jigs, Telecom, Lighting, Medical devices, Photographic devices, Robots, Sculptures, Sound equipment, Sporting equipment, Tooling, Toys and more. 


What Can we help you do next?

∇ Go To Homepage For Die Casting China

→Casting Parts-Find out what we have done.

→Ralated Tips About Die Casting Services


By Minghe Die Casting Manufacturer |Categories: Helpful Articles |Material Tags: , , , , , ,Bronze Casting,Casting Video,Company History,Aluminum Die Casting |Comments Off

MingHe Casting Advantage

  • Comprehensive Casting design software and skilled engineer enables sample to be done within 15-25 days
  • Complete set of inspection equipment & quality control makes excellent Die Casting products
  • A fine shipping process and good supplier guarantee we can always deliver Die Casting goods on time
  • From prototypes to end parts, upload your CAD files, fast and professional quote in 1-24 hours
  • Wide-ranging capabilities for designing prototypes or massive manufacturing end use Die Casting parts
  • Advanced Die Casting techniques (180-3000T Machine,Cnc Machining, CMM) process a variety of metal & plastic materials

HelpFul Articles

Rare earth can effectively improve the toughness of cast steel

As we all know, adding an appropriate amount of rare earth elements to steel materials will have a s

Control of Intergranular Corrosion of Austenitic Stainless Steel

Among the various corrosions of stainless steel, the intergranular corrosion accounts for about 10%.

Measures to reduce the content of hydrogen, oxygen and nitrogen in steel

Generally, clean steel refers to a steel grade that has a low content of five major impurity element

Research on the influence of hydrogen on the strength of steel

As we all know, the hydrogen in the material will be trapped at various trap positions (dislocations

One table to understand the heat treatment of steel products

One table to understand the heat treatment of steel products

Study on Mechanical Properties of Welded Joints of Duplex Stainless Steel

Duplex stainless steel has the same proportion of ferrite and austenite, and has excellent mechanica

Characteristics and uses of 24 commonly used mechanical die steels

1. 45-high-quality carbon structural steel, the most commonly used medium-carbon quenched and temper

The Failure Analysis of H13 Steel Die Casting Mould

Using optical microscope, scanning electron microscope, hardness tester, impact testing machine, etc

Effect of Drill and Nickel on the Thermal Damage Resistance of 4Cr5Mo2V Die Casting Die Steel

4Cr5 Mo2V is a commonly used die-casting die steel. In the process of die-casting aluminum alloy, du

The Comparison Of 7 Kinds Die Steel

It has high hardenability. Because 1.20%~1.60% (mass fraction) of tungsten is added to form carbides