The Anti-Corrosion Treatment Of Ductile Iron Pipe Fittings

Publish Time: Author: Site Editor Visit: 34287

The Anti-Corrosion Treatment Of Ductile Iron Pipe Fittings

1. Asphalt paint coating

Asphalt paint coating is used to transport gas pipelines. Preheating the pipe before painting can improve the adhesion of the asphalt paint and accelerate the drying.

2. Cement mortar lining + special coating

This kind of internal anti-corrosion measures is suitable for pipelines conveying sewage and can improve the corrosion resistance of the inner lining.

3. Epoxy coal pitch coating

The epoxy coal tar coating is suitable for both gas pipelines and sewage pipelines. It is a two-component coating that has high adhesion and a very smooth surface.

4. Epoxy ceramic lining

Epoxy ceramic lining is suitable for sewage pipelines and gas pipelines, but due to the difficult manufacturing process and high cost, it has certain limitations in use. Epoxy ceramic lining has high adhesion and smoothness, which is an excellent anti-corrosion.

5. Aluminate cement coating or sulfate cement coating

Both of these special cement coatings are suitable for the internal anti-corrosion of ductile iron pipes used in sewage pipelines to improve the corrosion resistance of the acid and alkali components in the sewage.

6. Polyurethane coating

It is a new type of green special coating developed to meet the needs of environmental protection. It has good wear resistance and corrosion resistance.


Please keep the source and address of this article for reprinting:The Anti-Corrosion Treatment Of Ductile Iron Pipe Fittings


Minghe Die Casting Company are dedicated to manufacture and provide quality and high performance Casting Parts(metal die casting parts range mainly include Thin-Wall Die Casting,Hot Chamber Die Casting,Cold Chamber Die Casting),Round Service(Die Casting Service,Cnc Machining,Mold Making,Surface Treatment).Any custom Aluminum die casting, magnesium or Zamak/zinc die casting and other castings requirements are welcome to contact us.

ISO90012015 AND ITAF 16949 CASTING COMPANY SHOP

Under the control of ISO9001 and TS 16949,All processes are carried out through hundreds of advanced die casting machines, 5-axis machines, and other facilities, ranging from blasters to Ultra Sonic washing machines.Minghe not only has advanced equipment but also have professional team of experienced engineers,operators and inspectors to make the customer’s design come true.

POWERFUL ALUMINUM DIE CASTING WITH ISO90012015

Contract manufacturer of die castings. Capabilities include cold chamber aluminum die casting parts from 0.15 lbs. to 6 lbs., quick change set up, and machining. Value-added services include polishing, vibrating, deburring, shot blasting, painting, plating, coating, assembly, and tooling. Materials worked with include alloys such as 360, 380, 383, and 413.

PERFECT ZINC DIE CASTING PARTS IN CHINA

Zinc die casting design assistance/concurrent engineering services. Custom manufacturer of precision zinc die castings. Miniature castings, high pressure die castings, multi-slide mold castings, conventional mold castings, unit die and independent die castings and cavity sealed castings can be manufactured. Castings can be manufactured in lengths and widths up to 24 in. in +/-0.0005 in. tolerance.  

ISO 9001 2015 certified manufacturer of die cast magnesium and mold manufacturing

ISO 9001: 2015 certified manufacturer of die cast magnesium, Capabilities include high-pressure magnesium die casting up to 200 ton hot chamber & 3000 ton cold chamber, tooling design, polishing, molding, machining, powder & liquid painting, full QA with CMM capabilities, assembly, packaging & delivery.

Minghe Casting Additional Casting Service-investment casting etc

ITAF16949 certified. Additional Casting Service Include investment casting,sand casting,Gravity Casting, Lost Foam Casting,Centrifugal Casting,Vacuum Casting,Permanent Mold Casting,.Capabilities include EDI, engineering assistance, solid modeling and secondary processing.

Casting Parts Application Case Studies

Casting Industries Parts Case Studies for: Cars, Bikes, Aircraft, Musical instruments, Watercraft, Optical devices, Sensors, Models, Electronic devices, Enclosures, Clocks, Machinery, Engines, Furniture, Jewelry, Jigs, Telecom, Lighting, Medical devices, Photographic devices, Robots, Sculptures, Sound equipment, Sporting equipment, Tooling, Toys and more. 


What Can we help you do next?

∇ Go To Homepage For Die Casting China

→Casting Parts-Find out what we have done.

→Ralated Tips About Die Casting Services


By Minghe Die Casting Manufacturer |Categories: Helpful Articles |Material Tags: , , , , , ,Bronze Casting,Casting Video,Company History,Aluminum Die Casting |Comments Off

MingHe Casting Advantage

  • Comprehensive Casting design software and skilled engineer enables sample to be done within 15-25 days
  • Complete set of inspection equipment & quality control makes excellent Die Casting products
  • A fine shipping process and good supplier guarantee we can always deliver Die Casting goods on time
  • From prototypes to end parts, upload your CAD files, fast and professional quote in 1-24 hours
  • Wide-ranging capabilities for designing prototypes or massive manufacturing end use Die Casting parts
  • Advanced Die Casting techniques (180-3000T Machine,Cnc Machining, CMM) process a variety of metal & plastic materials

HelpFul Articles

Optimization of heat treatment process for GH690 alloy pipe

The 690 alloy tube used for the steam generator heat transfer tube of nuclear power plant bears the

The Anti-Corrosion Treatment Of Ductile Iron Pipe Fittings

Asphalt paint coating is used to transport gas pipelines. Preheating the pipe before painting can im

The Effect Of Fine-Grained Band In 690 Alloy Forged Bar On The Structure Of Finished Pipe

Alloy 690 is a nickel-based corrosion-resistant alloy. It not only has excellent stress corrosion cr

The Anticorrosion Of Ductile Iron Pipe Zinc Layer

At present, nodular cast iron pipes use cement lining as the internal anti-corrosion form, and zinc

The Influence Of Overheating Environment On Austenitic Stainless Steel Pipe

Before it can be decomposed, the austenite is transformed into martensite until it is cooled below t

Anti-corrosion treatment method of branch pipe stand in steel plant

The various energy transmission pipelines laid by the steel plant are supported by pipeline supports

Medium frequency induction heating heat treatment method for steel pipe, petroleum oil well pipe and drill pipe

The present invention is an intermediate frequency induction heating heat treatment method for steel

The Practical Application Of Line Pipe With Good Buckling Resistance

When the foundation of earthquake zone and tundra zone changes, pipelines laid in the zone may buckl