Method of reducing total oxygen in slab

Publish Time: Author: Site Editor Visit: 37376


Improving the cleanliness of the cast slab is the basis for the production of high-quality steel, and the total oxygen content of the cast slab is an important measure of the cleanliness of the molten steel. Reducing the total oxygen content of the cast slab is mainly carried out from three aspects: converter process, refining process and continuous casting process:
  1, converter process

   The converter process should implement high carbon pull rate and optimize the slag washing process.

  (1) End pull carbon

  Implement a less slag process, which strengthens the dephosphorization effect in the early stage, stabilizes the decarburization operation in the later stage, and then implements high-carbon control.

  (2) Slag washing process

   Promote the converter lime slag washing process, that is, during the converter tapping process, after the alloy is added, lime is directly added from the silo to the ladle along with the molten steel flow. This helps lime pre-melting in advance, promotes the slag to absorb inclusions for more time, and the initial slag can effectively cover the molten steel interface, reducing the probability of exposed molten steel to absorb oxygen.

  2, refining process

  The refining process should optimize the slag system, bottom argon blowing process, and calcium treatment process.

  (1) Slag system optimization

  The increase in the basicity of the slag is conducive to improving the deoxidizing capacity of the refining slag and reducing the oxygen content in the steel. At the same time, the slag should be reduced. This is because the SiO2 content in the slag is reduced, which greatly reduces the SiO2 activity coefficient, which can avoid or reduce the influence of the reaction between SiO2 in the slag and Al in the steel on the deoxidation of molten steel.

  (2) Optimize the bottom blowing argon process

   is mainly: (1) The entire refining process should use as little strong stirring as possible to reduce the exposure of molten steel and slag entrapment, and reduce the erosion of the ladle refractory material. (2) During the soft blowing process, pay attention to adjusting the argon gas so that the slag creeps, and the molten steel level is not exposed. (3) Before the VD reaches high vacuum, avoid excessive argon flow to expose molten steel; when reaching high vacuum, adjust the argon flow appropriately to ensure sufficient vacuum degassing effect and increase the reaction rate of slag steel.

  (3) Calcium treatment process

  Solid core pure calcium wire has obvious effect on Al2O3 inclusion denaturation. The calcium treatment process uses solid core pure calcium wire instead of silicon calcium and calcium iron cored wire.

  3, continuous casting process

The continuous casting process mainly protects the pouring: argon replacement is used before pouring, and asbestos bowl gaskets are used for the large package casing to avoid secondary oxidation caused by oxygen absorption in the molten steel; the addition of the covering agent for the tundish must meet the requirements to ensure that the molten steel is not exposed and the slag layer No crusting; strengthen the monitoring and maintenance of the automatic monitoring system for slag under the ladle to ensure the normal operation of the system; ensure that the drainage sand is added to increase the self-opening rate of the pouring slide.


Please keep the source and address of this article for reprinting: Method of reducing total oxygen in slab


Minghe Die Casting Company are dedicated to manufacture and provide quality and high performance Casting Parts(metal die casting parts range mainly include Thin-Wall Die Casting,Hot Chamber Die Casting,Cold Chamber Die Casting),Round Service(Die Casting Service,Cnc Machining,Mold Making,Surface Treatment).Any custom Aluminum die casting, magnesium or Zamak/zinc die casting and other castings requirements are welcome to contact us.

ISO90012015 AND ITAF 16949 CASTING COMPANY SHOP

Under the control of ISO9001 and TS 16949,All processes are carried out through hundreds of advanced die casting machines, 5-axis machines, and other facilities, ranging from blasters to Ultra Sonic washing machines.Minghe not only has advanced equipment but also have professional team of experienced engineers,operators and inspectors to make the customer’s design come true.

POWERFUL ALUMINUM DIE CASTING WITH ISO90012015

Contract manufacturer of die castings. Capabilities include cold chamber aluminum die casting parts from 0.15 lbs. to 6 lbs., quick change set up, and machining. Value-added services include polishing, vibrating, deburring, shot blasting, painting, plating, coating, assembly, and tooling. Materials worked with include alloys such as 360, 380, 383, and 413.

PERFECT ZINC DIE CASTING PARTS IN CHINA

Zinc die casting design assistance/concurrent engineering services. Custom manufacturer of precision zinc die castings. Miniature castings, high pressure die castings, multi-slide mold castings, conventional mold castings, unit die and independent die castings and cavity sealed castings can be manufactured. Castings can be manufactured in lengths and widths up to 24 in. in +/-0.0005 in. tolerance.  

ISO 9001 2015 certified manufacturer of die cast magnesium and mold manufacturing

ISO 9001: 2015 certified manufacturer of die cast magnesium, Capabilities include high-pressure magnesium die casting up to 200 ton hot chamber & 3000 ton cold chamber, tooling design, polishing, molding, machining, powder & liquid painting, full QA with CMM capabilities, assembly, packaging & delivery.

Minghe Casting Additional Casting Service-investment casting etc

ITAF16949 certified. Additional Casting Service Include investment casting,sand casting,Gravity Casting, Lost Foam Casting,Centrifugal Casting,Vacuum Casting,Permanent Mold Casting,.Capabilities include EDI, engineering assistance, solid modeling and secondary processing.

Casting Parts Application Case Studies

Casting Industries Parts Case Studies for: Cars, Bikes, Aircraft, Musical instruments, Watercraft, Optical devices, Sensors, Models, Electronic devices, Enclosures, Clocks, Machinery, Engines, Furniture, Jewelry, Jigs, Telecom, Lighting, Medical devices, Photographic devices, Robots, Sculptures, Sound equipment, Sporting equipment, Tooling, Toys and more. 


What Can we help you do next?

∇ Go To Homepage For Die Casting China

→Casting Parts-Find out what we have done.

→Ralated Tips About Die Casting Services


By Minghe Die Casting Manufacturer |Categories: Helpful Articles |Material Tags: , , , , , ,Bronze Casting,Casting Video,Company History,Aluminum Die Casting |Comments Off

MingHe Casting Advantage

  • Comprehensive Casting design software and skilled engineer enables sample to be done within 15-25 days
  • Complete set of inspection equipment & quality control makes excellent Die Casting products
  • A fine shipping process and good supplier guarantee we can always deliver Die Casting goods on time
  • From prototypes to end parts, upload your CAD files, fast and professional quote in 1-24 hours
  • Wide-ranging capabilities for designing prototypes or massive manufacturing end use Die Casting parts
  • Advanced Die Casting techniques (180-3000T Machine,Cnc Machining, CMM) process a variety of metal & plastic materials

HelpFul Articles

Method of reducing total oxygen in slab

Improving the cleanliness of the cast slab is the basis for the production of high-quality steel, an

Summary of changing factors and control methods of blast furnace type

The normal blast furnace operation type is characterized by smooth inner wall surface and stable sla

Plastical Forming Method Of Magnesium Alloy

Due to its high production efficiency, low cost, and the ability to produce products with more compl

The Calculation Method Of Mold Making Price

Empirical calculation method mold price = material cost + design cost + processing cost and profit +

The Improvement Method Of Mold Performance

In addition to the reasonable coordination of the matrix with sufficiently high strength and toughne

The Maintenance Method Of Die Casting Mold

Die casting die belongs to a kind of casting liquid die forging and special die casting die forging

The Water Filling Method Of Centrifugal Pump

Centrifugal pumps (except self-priming pumps) must be filled with water before starting the pump and

Methods And Steps Of Stamping Die Design

There are many types of molds, which can be divided into: ①Metal molds based on processing goals and

The Disassembly Method Of Mechanical Parts

The disassembly of mechanical parts is related to the safety of the parts and the efficiency of disa

Surface and internal quality inspection methods of castings

The inspection of castings mainly includes size inspection, visual inspection of appearance and surf