New Die Casting Tooling Acceptance Content

Publish Time: Author: Site Editor Visit: 14565

When the new die-casting mold is in place, because there is no corresponding understanding of all aspects of its performance, it is necessary to confirm the following content during acceptance.

  1. Is the mold number clear and correct?
  2. Mold size?
  3. What is the diameter of the material cylinder?
  4. What is the eccentricity under the mold?
  5. What is the spacing of the ejector holes?
  6. What is the size and spacing of the tie rod holes?
  7. Mold cavity error value ≤ 0.1mm (check the indentation around the cavity)?
  8. Surface roughness Ra≤0.4μm?
  9. There are no damages, scratches or cracks on the surface of the cavity?
  10.  Can the thimble and slider be free from jamming?
  11. The movable and fixed mold core is 0.02~0.06mm higher than the mold base?
  12. Is the arrangement of the ring holes on the mold base, top plate, thimble fixing plate and mold foot reasonable and convenient?
  13. Are the cooling water inlet and outlet marked clearly?
  14. Does the cooling water mold end interface match the specifications of the company’s common water pipes?
  15. Does the hydraulic cylinder mold end interface match the specifications of the company's common oil pipe interface?
  16. Does the supplier provide tie rods and top rods?
  17. Does the supplier provide core spare parts?
  18. Does the supplier provide spare parts drawings?
  19. Does the supplier provide the material certificate and heat treatment report?

MingHe Casting Advantage

  • Comprehensive Casting design software and skilled engineer enables sample to be done within 15-25 days
  • Complete set of inspection equipment & quality control makes excellent Die Casting products
  • A fine shipping process and good supplier guarantee we can always deliver Die Casting goods on time
  • From prototypes to end parts, upload your CAD files, fast and professional quote in 1-24 hours
  • Wide-ranging capabilities for designing prototypes or massive manufacturing end use Die Casting parts
  • Advanced Die Casting techniques (180-3000T Machine,Cnc Machining, CMM) process a variety of metal & plastic materials

HelpFul Articles

How To Calculate Pressure Die Casting Tonnage

Calculation Formula The calculation formula for the selection of die-casting machine: Die-casting m

The Numerical Control Cutting Process Of Thread

The thread cutting process depends on the structure of the machined parts and the CNC machine tool u

Approximate Fitting And NC Machining Of Ellipse Gear

Oval gears are widely used in automatic machinery and instrument industries, and are a type of non-c

The Role And Application Field Of The Cylinder Telescopic Sheath

The cylinder telescopic sheath is a protective component that is installed on the oil cylinder, cyli

The Wavelet Analysis Of Overcut In Free-Form Surfaces CNC Machining

The manufacturing cycle is long. Operators are prone to fatigue. Once a failure occurs, it often tak

Using pure oxygen burner to reduce energy consumption of ladle preheating

The Wu Steel Works has two workshops, one steelmaking workshop and the second steelmaking workshop.